MOQ: | 100pcs |
Price: | As negotiation |
Standard Packaging: | cartons,pallets |
Delivery Period: | 20-25days |
Payment Method: | T/T L/C |
Supply Capacity: | 100 tons per month for NdFeB magnet |
Attribute | Value |
---|---|
Grade | N35-N52 |
Application | Widely Used |
Size | Customized |
Material | Neodymium |
Magnetic Flux Density | High |
Coating | Nickel |
Magnetic Field Strength | High |
Parameter Name | Parameter Values | Unit |
---|---|---|
Curie Temperature | 310~380 | ℃ |
Relative Recoil Permeability | 1.02~1.05 | |
Reversible Temperature Coefficient of Br (20~100℃) | -0.09~-0.13 | %/℃ |
Reversible Temperature Coefficient of Hcj (20~100℃) | -0.4~-0.7 | %/℃ |
Density | 7.50~7.70 | g/cm3 |
Vickers Hardness | 550~700 | |
Bending Strength | -0.09~-0.13 | MPa |
Tensile Strength | ≥80 | MPa |
Compressive Strength | 800 ~1050 | MPa |
Electric Resistivity | 150 | μΩ·cm |
Thermal Conductivity | 8~10 | W/(M·℃) |
Attributes | Specifications |
---|---|
Magnetic Performance | Stable |
Magnetic Field Strength | High |
Shape | Sintered |
Temperature Resistance | High |
Coating | Nickel |
Corrosion Resistance | High |
Size | Customized |
Material | Neodymium-Iron-Boron Magnetic-Alloy-Compound |
Grade | N35-N52 |
Magnetic Flux Density | High |
MOQ: | 100pcs |
Price: | As negotiation |
Standard Packaging: | cartons,pallets |
Delivery Period: | 20-25days |
Payment Method: | T/T L/C |
Supply Capacity: | 100 tons per month for NdFeB magnet |
Attribute | Value |
---|---|
Grade | N35-N52 |
Application | Widely Used |
Size | Customized |
Material | Neodymium |
Magnetic Flux Density | High |
Coating | Nickel |
Magnetic Field Strength | High |
Parameter Name | Parameter Values | Unit |
---|---|---|
Curie Temperature | 310~380 | ℃ |
Relative Recoil Permeability | 1.02~1.05 | |
Reversible Temperature Coefficient of Br (20~100℃) | -0.09~-0.13 | %/℃ |
Reversible Temperature Coefficient of Hcj (20~100℃) | -0.4~-0.7 | %/℃ |
Density | 7.50~7.70 | g/cm3 |
Vickers Hardness | 550~700 | |
Bending Strength | -0.09~-0.13 | MPa |
Tensile Strength | ≥80 | MPa |
Compressive Strength | 800 ~1050 | MPa |
Electric Resistivity | 150 | μΩ·cm |
Thermal Conductivity | 8~10 | W/(M·℃) |
Attributes | Specifications |
---|---|
Magnetic Performance | Stable |
Magnetic Field Strength | High |
Shape | Sintered |
Temperature Resistance | High |
Coating | Nickel |
Corrosion Resistance | High |
Size | Customized |
Material | Neodymium-Iron-Boron Magnetic-Alloy-Compound |
Grade | N35-N52 |
Magnetic Flux Density | High |