Attribute | Value |
---|---|
Application | Generator, Microphone, Measuring Instrument |
Magnetization Direction | Axial, Radial, Multi-poles |
BHmax | 1.13-9 MGOe |
Tolerance | ±0.05mm |
Grade | Alnico 5,8 Is Normally Used |
Hcj | ≥30 KA/m |
Max Operating Temperature | 550℃ |
Material | Cast Alnico |
Grade | Remanence (Br) | Intrinsic Coercivity (Hcj) | Maximum Energy Product | Max Temp |
---|---|---|---|---|
Alnico 3 | 520 mT | 43 KA/m | 1.0-1.25 MGOe | 450℃ |
Alnico 5 | 1100 mT | 51 KA/m | 3.5-4.15 MGOe | 525℃ |
Alnico 8 | 780 mT | 106 KA/m | 3.9-4.5 MGOe | 550℃ |
Alnico 8HC | 680 mT | 151 KA/m | 4.1-4.5 MGOe | 550℃ |
MOQ: | 100pcs |
Price: | As negotiation |
Standard Packaging: | cartons,pallets |
Delivery Period: | 20-25days |
Payment Method: | T/T L/C |
Supply Capacity: | 20 tons per month for SmCo magnet |
Attribute | Value |
---|---|
Application | Generator, Microphone, Measuring Instrument |
Magnetization Direction | Axial, Radial, Multi-poles |
BHmax | 1.13-9 MGOe |
Tolerance | ±0.05mm |
Grade | Alnico 5,8 Is Normally Used |
Hcj | ≥30 KA/m |
Max Operating Temperature | 550℃ |
Material | Cast Alnico |
Grade | Remanence (Br) | Intrinsic Coercivity (Hcj) | Maximum Energy Product | Max Temp |
---|---|---|---|---|
Alnico 3 | 520 mT | 43 KA/m | 1.0-1.25 MGOe | 450℃ |
Alnico 5 | 1100 mT | 51 KA/m | 3.5-4.15 MGOe | 525℃ |
Alnico 8 | 780 mT | 106 KA/m | 3.9-4.5 MGOe | 550℃ |
Alnico 8HC | 680 mT | 151 KA/m | 4.1-4.5 MGOe | 550℃ |