| MOQ: | 100pcs |
| Price: | As negotiation |
| Standard Packaging: | cartons,pallets |
| Delivery Period: | 20-25days |
| Payment Method: | T/T L/C |
| Supply Capacity: | 20 tons per month for SmCo magnet |
| Attribute | Value |
|---|---|
| Operating Temperature | 250-500°C |
| Material | Samarium Cobalt |
| Application | Spaceflight, National Defense, Microwave, Sensors |
| Grade | YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 |
| Magnetization | Through Axial, Thickness Or Customized |
| Coating | Uncoated |
| Grade | Remanence(Br) | Coercivity(Hcb) | Intrinsic Coercivity(Hcj) | Max Energy Product(BH)max | Curie Temperature(TC) | Max Work Temp(TW) | Temperature Coefficient of Br(Br) | Temperature Coefficient of Hcj(Hcj) |
|---|---|---|---|---|---|---|---|---|
| YXG-24H | 0.95-1.02 | 692-764 | ≥1990 | 22-24 | 800 | 350 | -0.025 | -0.20 |
| YXG-26H | 1.02-1.05 | 748-796 | ≥1990 | 24-26 | 800 | 350 | -0.030 | -0.20 |
| YXG-28H | 1.03-1.08 | 756-812 | ≥1990 | 26-28 | 800 | 350 | -0.035 | -0.20 |
| YXG-30H | 1.08-1.10 | 788-835 | ≥1990 | 28-30 | 800 | 350 | -0.035 | -0.20 |
| YXG-32H | 1.10-1.13 | 812-860 | ≥1990 | 29-32 | 800 | 350 | -0.035 | -0.20 |
| Parameter Name | Unit | SmCo5 | Sm2Co17 |
|---|---|---|---|
| Density | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
| Curie Temperature | ℃ | 700 ~ 750 | 800 ~ 850 |
| Max. Operating Temperature | ℃ | 250 | 350 |
| Temperature Coefficient Of Br | %/℃ | -0.05 | -0.03 |
| Vickers Hardness | HV | 450 ~ 500 | 550 ~600 |
| Electronic Resistivity | Ω.cm | 5 ~ 6 x 10(-5) | 8 ~ 9 x 10(-5) |
| Thermal Conductivity | W/mK | 12 | 13 |
| MOQ: | 100pcs |
| Price: | As negotiation |
| Standard Packaging: | cartons,pallets |
| Delivery Period: | 20-25days |
| Payment Method: | T/T L/C |
| Supply Capacity: | 20 tons per month for SmCo magnet |
| Attribute | Value |
|---|---|
| Operating Temperature | 250-500°C |
| Material | Samarium Cobalt |
| Application | Spaceflight, National Defense, Microwave, Sensors |
| Grade | YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 |
| Magnetization | Through Axial, Thickness Or Customized |
| Coating | Uncoated |
| Grade | Remanence(Br) | Coercivity(Hcb) | Intrinsic Coercivity(Hcj) | Max Energy Product(BH)max | Curie Temperature(TC) | Max Work Temp(TW) | Temperature Coefficient of Br(Br) | Temperature Coefficient of Hcj(Hcj) |
|---|---|---|---|---|---|---|---|---|
| YXG-24H | 0.95-1.02 | 692-764 | ≥1990 | 22-24 | 800 | 350 | -0.025 | -0.20 |
| YXG-26H | 1.02-1.05 | 748-796 | ≥1990 | 24-26 | 800 | 350 | -0.030 | -0.20 |
| YXG-28H | 1.03-1.08 | 756-812 | ≥1990 | 26-28 | 800 | 350 | -0.035 | -0.20 |
| YXG-30H | 1.08-1.10 | 788-835 | ≥1990 | 28-30 | 800 | 350 | -0.035 | -0.20 |
| YXG-32H | 1.10-1.13 | 812-860 | ≥1990 | 29-32 | 800 | 350 | -0.035 | -0.20 |
| Parameter Name | Unit | SmCo5 | Sm2Co17 |
|---|---|---|---|
| Density | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
| Curie Temperature | ℃ | 700 ~ 750 | 800 ~ 850 |
| Max. Operating Temperature | ℃ | 250 | 350 |
| Temperature Coefficient Of Br | %/℃ | -0.05 | -0.03 |
| Vickers Hardness | HV | 450 ~ 500 | 550 ~600 |
| Electronic Resistivity | Ω.cm | 5 ~ 6 x 10(-5) | 8 ~ 9 x 10(-5) |
| Thermal Conductivity | W/mK | 12 | 13 |