Parameter | Value | Unit |
---|---|---|
Curie Temperature | 310~380 | ℃ |
Density | 7.50~7.70 | g/cm³ |
Vickers Hardness | 550~700 | |
Tensile Strength | ≥80 | MPa |
Compressive Strength | 800 ~1050 | MPa |
Thermal Conductivity | 8~10 | W/(M·℃) |
Step | Description |
---|---|
1. Mixing | Mix the ingredients |
2. Melting | Dissolve mixture at high temperature to prepare alloy |
3. Fine Pulverization | Turn alloy into fine powder |
4. Molding | Press powder with applied magnetic field |
5. Sintering | Sinter at ~1,100℃ with heat treatment at ~600℃ |
6. Processing | Finish into product shape |
7. Surface Treatment | Apply rustproof coating |
8. Magnetization | Apply magnetic field to activate magnetism |
MOQ: | 100pcs |
Price: | As negotiation |
Standard Packaging: | cartons,pallets |
Delivery Period: | 20-25days |
Payment Method: | T/T L/C |
Supply Capacity: | 100 tons per month for NdFeB magnet |
Parameter | Value | Unit |
---|---|---|
Curie Temperature | 310~380 | ℃ |
Density | 7.50~7.70 | g/cm³ |
Vickers Hardness | 550~700 | |
Tensile Strength | ≥80 | MPa |
Compressive Strength | 800 ~1050 | MPa |
Thermal Conductivity | 8~10 | W/(M·℃) |
Step | Description |
---|---|
1. Mixing | Mix the ingredients |
2. Melting | Dissolve mixture at high temperature to prepare alloy |
3. Fine Pulverization | Turn alloy into fine powder |
4. Molding | Press powder with applied magnetic field |
5. Sintering | Sinter at ~1,100℃ with heat treatment at ~600℃ |
6. Processing | Finish into product shape |
7. Surface Treatment | Apply rustproof coating |
8. Magnetization | Apply magnetic field to activate magnetism |