| Jumlah Pesanan Minimum: | 100 PCS |
| Harga: | As negotiation |
| kemasan standar: | karton, palet |
| Periode pengiriman: | 20-25 hari |
| metode pembayaran: | T/TL/C |
| Kapasitas Pasokan: | 20 ton per bulan untuk magnet SmCo |
| Atribut | Nilai |
|---|---|
| Material | Samarium Cobalt |
| Aplikasi | Penerbangan Luar Angkasa, Pertahanan Nasional, Gelombang Mikro, Sensor |
| Suhu Operasi | 250-500°C |
| Magnetisasi | Melalui Aksial, Ketebalan Atau Disesuaikan |
| Grade | YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 |
| Pelapisan | Tidak Dilapisi |
| Grade | Remanensi(Br) | Koersivitas(Hcb) | Koersivitas Intrinsic(Hcj) | Produk Energi Maks(BH)max | Suhu Curie(TC) | Suhu Kerja Maks(TW) | Koefisien Suhu Br(Br) | Koefisien Suhu Hcj(Hcj) |
|---|---|---|---|---|---|---|---|---|
| YXG-24H | 0.95-1.02 | 692-764 | ≥1990 | 175-191 | 800 | 350 | -0.025 | -0.20 |
| YXG-26H | 1.02-1.05 | 748-796 | ≥1990 | 191-207 | 800 | 350 | -0.030 | -0.20 |
| YXG-28H | 1.03-1.08 | 756-812 | ≥1990 | 207-220 | 800 | 350 | -0.035 | -0.20 |
| YXG-30H | 1.08-1.10 | 788-835 | ≥1990 | 220-240 | 800 | 350 | -0.035 | -0.20 |
| YXG-32H | 1.10-1.13 | 812-860 | ≥1990 | 230-255 | 800 | 350 | -0.035 | -0.20 |
| Nama Parameter | Satuan | SmCo5 | Sm2Co17 |
|---|---|---|---|
| Kepadatan | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
| Suhu Curie | ℃ | 700 ~ 750 | 800 ~ 850 |
| Suhu Operasi Maks. | ℃ | 250 | 350 |
| Koefisien Suhu Br | %/℃ | -0.05 | -0.03 |
| Kekerasan Vickers | HV | 450 ~ 500 | 550 ~600 |
| Jumlah Pesanan Minimum: | 100 PCS |
| Harga: | As negotiation |
| kemasan standar: | karton, palet |
| Periode pengiriman: | 20-25 hari |
| metode pembayaran: | T/TL/C |
| Kapasitas Pasokan: | 20 ton per bulan untuk magnet SmCo |
| Atribut | Nilai |
|---|---|
| Material | Samarium Cobalt |
| Aplikasi | Penerbangan Luar Angkasa, Pertahanan Nasional, Gelombang Mikro, Sensor |
| Suhu Operasi | 250-500°C |
| Magnetisasi | Melalui Aksial, Ketebalan Atau Disesuaikan |
| Grade | YXG-26H, YXG-30H, YXG-28, YXG-30, YXG-32 |
| Pelapisan | Tidak Dilapisi |
| Grade | Remanensi(Br) | Koersivitas(Hcb) | Koersivitas Intrinsic(Hcj) | Produk Energi Maks(BH)max | Suhu Curie(TC) | Suhu Kerja Maks(TW) | Koefisien Suhu Br(Br) | Koefisien Suhu Hcj(Hcj) |
|---|---|---|---|---|---|---|---|---|
| YXG-24H | 0.95-1.02 | 692-764 | ≥1990 | 175-191 | 800 | 350 | -0.025 | -0.20 |
| YXG-26H | 1.02-1.05 | 748-796 | ≥1990 | 191-207 | 800 | 350 | -0.030 | -0.20 |
| YXG-28H | 1.03-1.08 | 756-812 | ≥1990 | 207-220 | 800 | 350 | -0.035 | -0.20 |
| YXG-30H | 1.08-1.10 | 788-835 | ≥1990 | 220-240 | 800 | 350 | -0.035 | -0.20 |
| YXG-32H | 1.10-1.13 | 812-860 | ≥1990 | 230-255 | 800 | 350 | -0.035 | -0.20 |
| Nama Parameter | Satuan | SmCo5 | Sm2Co17 |
|---|---|---|---|
| Kepadatan | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
| Suhu Curie | ℃ | 700 ~ 750 | 800 ~ 850 |
| Suhu Operasi Maks. | ℃ | 250 | 350 |
| Koefisien Suhu Br | %/℃ | -0.05 | -0.03 |
| Kekerasan Vickers | HV | 450 ~ 500 | 550 ~600 |